MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco RPM® NLGI 1 Arctic Grease
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Chevron RPM Arctic Grease is a premium quality grease.

It is manufactured using a polyurea acetate complex thickener, special low viscosity base oil, and rust and oxidation inhibitors. It is black in color and its texture is smooth and buttery.

It is specially formulated for use in automotive and industrial applications where extreme low temperatures are encountered.

Chevron RPM Arctic Grease has outstanding low temperature lubrication qualities and provides metal parts with excellent rust and corrosion protection as well as protection from wear.

Applications

Chevron RPM Arctic Grease is recommended as a premium general purpose automotive and industrial grease where extreme low temperature performance is required.

It is also recommended for use in environments with a wide temperature range.

It is approved for the NLGI Certification Mark GC LB.

Key Words: CPS Number: 259131; MSDS Number: 4727
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 101Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 115 SUS
Saybolt Viscosity at 210°F 40.7 SUS
Kinematic Viscosity at 40°C (104°F) 22 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 4.3 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Penetration 325Worked
Penetration P(0), 1/10 mm 310
Timken Test 45.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -50.0 °C
Pour Point -27.0 °CASTM D97
Flash Point 176 °CASTM D92
Dropping Point 245 °C
 
Descriptive Properties
ColorBlack
Lincoln Ventmeter, psig at 30 s, at 0°F100
Lincoln Ventmeter, psig at 30 s, at -22°F420
Lincoln Ventmeter, psig at 30 s, at 30°F0
Lincoln Ventmeter, psig at 30 s, at 75°F0
TextureSmooth, Buttery
Thickener, % / type16 / Polyurea Complex

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV258 / 74873

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.