MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Estane® ZHF 78AT0 Thermoplastic Polyurethane, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Type: Estane® ZHF 78AT0 NAT021 is a soft, polyether based, NHFR thermoplastic polyurethane (TPU) compound.

Features: Soft, transparent, flame retardant.

Uses: Wire and Cable

Available in Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccISO 2781
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 78
@Time 3.00 sec
ISO 868
Tensile Strength, Ultimate 30.1 MPaISO 527
Elongation at Break 670 %ISO 527
50% Modulus 0.00350 GPa
@Strain 50 %
100% Modulus 0.00450 GPa
@Strain 100 %
300% Modulus 0.00750 GPa
@Strain 300 %
Tear Strength 85.2 kN/mWithout Nick; ISO 34-1B
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Zone 1 160 °C
Zone 2 175 °C
Zone 3 180 °C
Zone 4 190 °C
Adapter Temperature 185 °C
Die Temperature 175 °Ctip
 180 °C
 180 °C
Drying Temperature 104 °C
Dry Time 3.00 hour
Dew Point -40.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant

PNOVEON596 / 121487

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.