System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LG Chemical KEYFLEX BT GN7142F Ester Type TPE
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyester, TP
;
Polyester Thermoplastic Elastomer
Material Notes:
Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Low Modulus
Application: Cable & Wire Jackets, Hose & Tubing, Sheet
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.20
g/cc
ASTM D792
Maximum Moisture Content
0.010
Injection Molding
0.010
Extrusion Molding
Melt Flow
10
g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore D
42
ASTM D2240
Tensile Strength at Break
11.8
MPa
@Thickness 2.00 mm
50mm/min; ASTM D638
Elongation at Break
350 %
@Thickness 2.00 mm
50mm/min; ASTM D638
Izod Impact, Notched
NB
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
NB
@Thickness 6.40 mm,
Temperature -40.0 °C
ASTM D256
Electrical Properties
Original Value
Comments
Dielectric Strength
24.0
kV/mm
@Thickness 1.00 mm
ASTM D149
Thermal Properties
Original Value
Comments
Melting Point
190
°C
Peak
Processing Properties
Original Value
Comments
Rear Barrel Temperature
190
-
210
°C
Injection Molding
Middle Barrel Temperature
200
-
220
°C
Injection Molding
Front Barrel Temperature
210
-
230
°C
Injection Molding
Nozzle Temperature
210
-
230
°C
Injection Molding
Zone 1
190
-
210
°C
Extrusion Molding
Zone 2
200
-
220
°C
Extrusion Molding
Zone 3
205
-
225
°C
Extrusion Molding
Zone 4
210
-
230
°C
Extrusion Molding
Adapter Temperature
210
-
230
°C
Extrusion Molding
Die Temperature
200
-
240
°C
Extrusion Molding
Melt Temperature
190
-
230
°C
Injection Molding
190
-
230
°C
Extrusion Molding
Mold Temperature
20.0
-
40.0
°C
Injection Molding
Drying Temperature
80.0
-
90.0
°C
Injection Molding
80.0
-
90.0
°C
Extrusion Molding
Dry Time
3.00
-
4.00
hour
Injection Molding
3.00
-
4.00
hour
Extrusion Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Envalior Arnitel® UM551-V TPC-ES FR, Flame Retardant
Envalior Arnitel® UM551-V Polyether Ester Elastomer (European Grade)
Envalior Arnitel® UM551-V 55 Shore D, Flame Retardant (halogen-, phosphorous-free) Copolyester Elastomer (North America)
LG Chemical KEYFLEX BT 2140D Ester Type TPE
LG Chemical KEYFLEX BT 3028D Ester Type TPE
PLAY442 / 148452
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.