MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Materion Beryllium Copper Alloy 25 Rod and Tube DSTO-2 (C17200)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Alloy 25 DSTO rod and tube from Materion provides an optimal combination of strength and ductility. This alloy features high thermal stability, so the mechanical properties will not degrade over time in high-temperature, downhole environments. It is a highly resilient alloy which also features high fatigue strength and magnetic permeability approaching unity. Alloy 25 DSTO also shows good resistance to wear, galling, corrosion, sulfide stress cracking and chloride stress corrosion cracking. Typical applications include flex shafts, flex collars and couplings for oil and gas exploration.

Information provided by Materion.

Key Words: ASTM B740
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.36 g/cc0.302 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C >= 26.0>= 26.0
Tensile Strength, Ultimate >= 931 MPa>= 135000 psi
Tensile Strength, Yield >= 689 MPa
@Strain 0.200 %
>= 100000 psi
@Strain 0.200 %
Elongation at Break >= 12.0 %>= 12.0 %
Modulus of Elasticity 131 GPa19000 ksi
Poissons Ratio 0.3000.300
Shear Modulus 73.0 GPa10600 ksiCalculated
Charpy Impact 14.9 J11.0 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000570 - 0.00000690 ohm-cm0.00000570 - 0.00000690 ohm-cm
Magnetic Permeability <= 1.0006<= 1.0006
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 105 W/m-K729 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Co + Ni >= 0.200 %>= 0.200 %
Co + Ni + Fe <= 0.600 %<= 0.600 %
Copper, Cu 97.4 - 98.0 %97.4 - 98.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBB610ab / 323500

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.