MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LEXAN™ Copolymer EXL6414 Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.

Features: High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.150 %0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %0.35 %ISO 62-1
Viscosity 7.0 cP
@Load 1.20 kg,
Temperature 300 °C
7.0 cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 8.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
8.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 58.0 MPa8410 psi50 mm/min; ISO 527
 59.0 MPa8560 psi50 mm/min; ASTM D638
Tensile Strength, Yield 54.0 MPa7830 psi50 mm/min; ISO 527
 55.0 MPa7980 psi50 mm/min; ASTM D638
Elongation at Break 88 %88 %50 mm/min; ISO 527
 100 %100 %50 mm/min; ASTM D638
Elongation at Yield 5.5 %5.5 %50 mm/min; ASTM D638
 6.0 %6.0 %50 mm/min; ISO 527
Tensile Modulus 1.72 GPa249 ksi50 mm/min; ASTM D638
 2.27 GPa329 ksi1 mm/min; ISO 527
Flexural Strength 79.0 MPa11500 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 85.0 MPa12300 psiyield, 2 mm/min; ISO 178
Flexural Modulus 1.99 GPa289 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.09 GPa303 ksi2 mm/min; ISO 178
Izod Impact Notched 801 J591 ft-lbASTM D256
 694 J
@Temperature -30.0 °C
512 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 32.04 J/cm60.02 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 70.0 kJ/m²33.3 ft-lb/in²80*10*3; ISO 180/1A
 60.0 kJ/m²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 7.00 J/cm²33.3 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 62.0 J45.7 ft-lbASTM D3763
 61.0 J
@Temperature -30.0 °C
45.0 ft-lb
@Temperature -22.0 °F
ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.70e+17 ohm-cm1.70e+17 ohm-cmIEC 60093
Surface Resistance 4.10e+17 ohm4.10e+17 ohmROA; IEC 60093
Dielectric Constant 2.6
@Frequency 1e+6 Hz
2.6
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm
@Thickness 3.20 mm
457 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor 0.0094
@Frequency 1e+6 Hz
0.0094
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  69.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.3 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
 70.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  72.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
40.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 73.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
40.6 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °C277 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 136 °C
@Thickness 3.20 mm
277 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C252 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 122 °C
@Thickness 3.20 mm
252 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 140 °C284 °FRate B/120; ISO 306
 141 °C286 °FRate B/50; ISO 306
 141 °C286 °FRate B/50; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 - 310 °C554 - 590 °F
Zone 2 280 - 305 °C536 - 581 °F
Zone 3 295 - 315 °C563 - 599 °F
Melt Temperature 295 - 315 °C563 - 599 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80211 / 288158

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.