MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik Vestodur® X7292 nf PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: Halogen and phosphate free, self-extinguishing PBT-Resin with higher flexibility for processing by extrusion.

Applications: Cable insulation.

ISO data as provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³
Water Absorption 0.00 %0.00 %
Melt Flow 12 g/10 min12 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.0 MPa4350 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 14 %14 %
Modulus of Elasticity 0.750 GPa109 ksi
Charpy Impact Unnotched NBNB
 9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+13 ohm1.00e+13 ohm
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear <= 50.0 µm/m-°C
@Temperature 20.0 °C
<= 27.8 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °F
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °F
Vicat Softening Point 190 °C374 °F50°C/hr/50 N
Flammability, UL94  V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestodur® 1003-FR5 Flame Retardant PBT
Evonik Vestodur® HI19-FR2 nf PBT
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
Evonik Vestodur® X7347 nf PBT

PHUM37 / 47470

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.