MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CMW® DSC Copper with Dispersed Aluminum Oxide  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Copper Alloy

Material Notes: CMW® DSC material is an extruded and cold worked powder metallurgy material consisting of copper and dispersed aluminum oxide. It has exceptional high temperature strength for its electrical conductivity both of which exceed the R.W.M.A Class 2 alloys.

CMW® DSC is used to its best advantage when welding coated steels, such as galvanized, electo-coated, aluminized, terne plate. It's ability to resist deformation over a long period, make it a top choice for such applications particularly where extended production runs (without cap change) are required.

Information provided by CMW Inc.

1

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 75
Tensile Strength, Ultimate 372 MPa
Tensile Strength, Yield 345 MPa
Elongation at Break 25 %
Reduction of Area 80 %
Modulus of Elasticity 123 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000203 ohm-cm85 % IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.0 µm/m-°C
@Temperature 100 °C
Thermal Conductivity 345 W/m-K
Melting Point 1080 °C
Softening Point 800 °CPermanent Softening
 
Component Elements PropertiesOriginal ValueComments
Al2O3 0.50 %
Copper, Cu 99.5 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
OMG Americas GlidCop® AL-15 Dispersion Strengthened Copper
AISI 1040 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
PD-135 Copper Chromium and Cadmium Alloy
ArcelorMittal MartINsite® 1200 Cold Rolled Steel
AISI 1030 Steel, as rolled

NCMW076 / 15889

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.