MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

TSRC T-BLEND® 3001-75N TPR/TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: T-BLEND® is a series of thermoplastic rubber compound materials produced by TSRC CORPORATION. T-BLEND® 3001-75N thermoplastic rubber has already widely used to replace conventional vulcanized rubber such as NBR, BR and SBR without vulcanization methods-T-BLEND® 3001-75N can be applied to a variety of unique products with excellent elasticity, flexibility and fine cells by injection molding process. T-BLEND® 3001-75N is a palletized elastomer compound based on styrenic block copolymer. T-BLEND® 3001-75N thermoplastic elastomer compound is recyclable including wastes from gate and runner. T-BLEND® 3001-75N thermoplastic rubber can meet vast requirements based on excellent weather durability, low temperature resistance, electricity insulation, chemical resistance and international heavy metal safety / RoHS Compliance.

Information provided by TSRC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 - 0.940 g/cc0.880 - 0.940 g/ccASTM D792
Melt Flow 10 - 40 g/10 min
@Load 5.00 kg,
Temperature 180 °C
10 - 40 g/10 min
@Load 11.0 lb,
Temperature 356 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 72 - 7872 - 78ASTM D2240
Tensile Strength 6.37 MPa925 psiType3, specimen; ASTM D412
Elongation at Break 250 %250 %500 mm/min; ASTM D412
Tear Strength 39.2 kN/m224 pliC Die; ASTM D624
 
Processing PropertiesMetricEnglishComments
Feed Temperature 160 °C320 °F
Rear Barrel Temperature 170 °C338 °F
Front Barrel Temperature 180 °C356 °F
Die Temperature 190 °C374 °F
Mold Temperature 30.0 - 40.0 °C86.0 - 104 °F
Drying Temperature 100 °C
@Time 3600 sec
212 °F
@Time 1.00 hour
hot air circulating oven/hopper
Back Pressure 0.343 - 0.676 MPa49.7 - 98.0 psi
Cycle Time - Injection 25 - 50 sec25 - 50 sec
 
Descriptive Properties
ColorNatural
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTSRC061 / 306349

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.