MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Westlake Mxsite LC78105-C Polyethylene Film, Using Energx Technology Services  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Mxsite LC78105-C polyethylene is recommended for the skin layers of blown stretch film. It will provide a very aggressive cling force in both a stretched and unstretched condition. The excellent cling force comes without a substantial increase in film unwind force. It is designed for machine wrap and hand wrap applications where good processability, low gel content and substantial cling are needed. It can be used as cling layer in many "one-sided cling" films because it clings very well to many non-cling resins.

Applications/Uses

  • Cast film
  • Films
  • Stretch film
  • Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Base Resin Density 0.915 g/cc0.0331 lb/in³ASTM D1505
    Thickness 20.3 microns0.799 milASTM D374
    Base Resin Melt Index 0.55 g/10 min0.55 g/10 minASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Film Tensile Strength at Yield, TD 9.70 MPa1410 psiASTM D882
    Film Elongation at Break, MD 450 %450 %ASTM D882
    Film Elongation at Break, TD 930 %930 %ASTM D882
    Elmendorf Tear Strength, MD 18.22 g/micron462.8 g/milASTM D1922
    Elmendorf Tear Strength, TD 45.81 g/micron1164 g/milASTM D1922
    Dart Drop 7.88 g/micron200 g/milASTM D1709A
    Film Tensile Strength at Break, MD 39.0 MPa5660 psiASTM D882
    Film Tensile Strength at Break, TD 36.0 MPa5220 psiASTM D882
    1% Secant Modulus, MD 187 MPa27100 psiASTM D882
    1% Secant Modulus, TD 244 MPa35400 psiASTM D882
     
    Optical PropertiesMetricEnglishComments
    Haze 3.3 %3.3 %ASTM D1003
    Gloss 83 %83 %at 45°; ASTM D2457
     
    Descriptive Properties
    Peel Cling, Aged 2 Weeks, 0%360 g
    Peel Cling, Aged 2 Weeks, 200%260 g

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services
    Westlake EC477AA Low Density Polyethylene
    Westlake EC476AA Low Density Polyethylene
    Westlake EC474AA Low Density Polyethylene
    Westlake EC472 Low Density Polyethylene

    PE9087 / 35143

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.