MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik EP 2325 Adhesion Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: A special purpose, medium hard polyester resign with a wide solubility and compatibility designed as a supplementary resin to improve the adhesion of numerous coating systems even on critical substrates

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.05 g/cc
@Temperature 23.0 °C
0.0379 lb/in³
@Temperature 73.4 °F
DIN 51 757
 1.24 g/cc
@Temperature 23.0 °C
0.0448 lb/in³
@Temperature 73.4 °F
DIN 53 479-B
Viscosity 500 cP
@Temperature 23.0 °C
500 cP
@Temperature 73.4 °F
DIN EN ISO 3219
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 1818[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesMetricEnglishComments
Softening Point 60.0 °C140 °FDIN 53 181
Glass Transition Temp, Tg 30.0 °C86.0 °FDIN 53 765
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 2.02.0DIN ISO 4630
 
Descriptive Properties
Hydroxyl Number (mg KOH/g)16DIN EN ISO 4629
Nonvolatile matter (%)60DIN EN ISO 3251

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUMB105 / 81107

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.