MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chesterton 660 Silicone Lubricant
Categories: Fluid; Lubricant; Silicone Base

Material Notes: Description: Chesterton® 660 Silicone Lubricant is a clean, clear, silicone fluid which will provide continuous film lubrication for mechanical parts and sliding surfaces constructed of plastic, rubber or metal . Wherever porous synthetics, plastics, rubber, neoprene, wood etc. come into contact with other materials, 660 Silicone Lubricant quickly penetrates surfaces to lubricate, prevent sticking and reduce wear. The product leaves a slippery, clean film which will not stain or leave gummy residues. It will stay where it is applied and not readily be squeezed out. Chesterton 660 Silicone Lubricant is quite versatile for both high and low temperature applications. The product is effective from -40°C to 205°C (-40°F to 400°F). It is invaluable as a lubricant where petroleum oils cannot be used.

Features:

  • Braod temperature range
  • NSF H1 - Registration number 133932 (bulk) and 133970 (aerosol)
  • Complies with FDA regulations for incidental food contact
  • Makes surface water resistant
  • Clean, non-staining
  • Penetrates fine tolerances
  • Long lasting

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.700 g/cc0.700 g/cc
Viscosity Measure 500 cSt500 cSt
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 205 °C401 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
AppearanceClear, colorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Overview of materials for Liquid Silicone Rubber
Shin-Etsu Silicones KF-6004 Fluid
Shin-Etsu Silicones 562P Fluid
Shin-Etsu Silicones 541 Fluid

PPTCHS081 / 138193

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.