MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Cera-Kote® 624A Cement
Categories: Ceramic; Oxide

Material Notes: Air-setting cement for use with a variety of insulating products. May be used for spray, dip, or brush application. The cement set with a strong hard film which will develop a ceramic bond above 1600°F (871°C).

Applications:

  • Adhesive to apply foils (stainless or aluminum) to fiber blanket and board
  • Adhesive to join vacuum formed ceramic fiber parts together
  • Adhesive and insulation for heating elements
  • Fiber surface encapsulation

Information provided by Morgan Advanced Materials

Key Words: Cement
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00140 GPa0.203 ksi
 
Thermal PropertiesMetricEnglishComments
Melting Point 1788 °C3250 °F
Maximum Service Temperature, Air <= 1204 °C<= 2199 °FContinuous Use
 
Processing PropertiesMetricEnglishComments
Drying Temperature <= 66.0 °C<= 151 °F
Shelf Life 6.00 Month6.00 Month
 
Component Elements PropertiesMetricEnglishComments
Al2O3 80 %80 %
Other 1.0 %1.0 %
SiO2 19 %19 %
 
Descriptive Properties
Classification Temperature (°C)1316
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6040 / 202824

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.