MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Radici RADILON® S HSX88 100 NT Nylon 6, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: PA6 injection molding grade. Toughened. Natural color. Suitable for parts requiring improved impact resistance

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: High impact or impact modified

Industries: Consumer Industry Goods, Transportation

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Water Absorption 8.8 %
@Thickness 2.00 mm
8.8 %
@Thickness 0.0787 in
Immersion at 23°C; ISO 62
Moisture Absorption 2.60 %
@Thickness 2.00 mm
2.60 %
@Thickness 0.0787 in
50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress  20.0 MPa
@Strain 0.75 %,
Temperature -20.0 °C
2900 psi
@Strain 0.75 %,
Temperature -4.00 °F
 20.0 MPa
@Strain 0.75 %,
Temperature 0.000 °C
2900 psi
@Strain 0.75 %,
Temperature 32.0 °F
 20.0 MPa
@Strain 1 %,
Temperature 23.0 °C
2900 psi
@Strain 1 %,
Temperature 73.4 °F
 20.0 MPa
@Strain 1.2 %,
Temperature 40.0 °C
2900 psi
@Strain 1.2 %,
Temperature 104 °F
 35.0 MPa
@Strain 3 %,
Temperature 40.0 °C
5080 psi
@Strain 3 %,
Temperature 104 °F
 40.0 MPa
@Strain 2 %,
Temperature 23.0 °C
5800 psi
@Strain 2 %,
Temperature 73.4 °F
 59.0 MPa
@Strain 3.8 %,
Temperature 23.0 °C
8560 psi
@Strain 3.8 %,
Temperature 73.4 °F
 60.0 MPa
@Strain 2.2 %,
Temperature 0.000 °C
8700 psi
@Strain 2.2 %,
Temperature 32.0 °F
 60.0 MPa
@Strain 2.1 %,
Temperature -20.0 °C
8700 psi
@Strain 2.1 %,
Temperature -4.00 °F
 72.0 MPa
@Strain 3.8 %,
Temperature 0.000 °C
10400 psi
@Strain 3.8 %,
Temperature 32.0 °F
 81.0 MPa
@Strain 5.0 %,
Temperature -20.0 °C
11700 psi
@Strain 5.0 %,
Temperature -4.00 °F
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527-2/1A
Elongation at Break >= 50 %>= 50 %Nominal, 50 mm/min; ISO 527-2/1A
Tensile Modulus 2.20 GPa319 ksi1mm/min; ISO 527-2/1A
Flexural Strength 80.0 MPa11600 psi2mm/min; ISO 178
Flexural Modulus 2.10 GPa305 ksi2mm/min; ISO 178
Secant Modulus  1.00 GPa
@Strain 3.75 %,
Temperature -40.0 °C
145 ksi
@Strain 3.75 %,
Temperature -40.0 °F
 1.99 GPa
@Strain 2.25 %,
Temperature 23.0 °C
289 ksi
@Strain 2.25 %,
Temperature 73.4 °F
 2.00 GPa
@Strain 3.75 %,
Temperature 0.000 °C
290 ksi
@Strain 3.75 %,
Temperature 32.0 °F
 2.00 GPa
@Strain 0.25 %,
Temperature 23.0 °C
290 ksi
@Strain 0.25 %,
Temperature 73.4 °F
 2.00 GPa
@Strain 4 %,
Temperature -20.0 °C
290 ksi
@Strain 4 %,
Temperature -4.00 °F
 2.10 GPa
@Strain 0.0 %,
Temperature -40.0 °C
305 ksi
@Strain 0.0 %,
Temperature -40.0 °F
 2.30 GPa
@Strain 0.0 %,
Temperature 23.0 °C
334 ksi
@Strain 0.0 %,
Temperature 73.4 °F
 2.40 GPa
@Strain 2 %,
Temperature -40.0 °C
348 ksi
@Strain 2 %,
Temperature -40.0 °F
 2.55 GPa
@Strain 3.75 %,
Temperature 23.0 °C
370 ksi
@Strain 3.75 %,
Temperature 73.4 °F
 2.60 GPa
@Strain 0.75 %,
Temperature -40.0 °C
377 ksi
@Strain 0.75 %,
Temperature -40.0 °F
 2.75 GPa
@Strain 2 %,
Temperature -20.0 °C
399 ksi
@Strain 2 %,
Temperature -4.00 °F
 2.75 GPa
@Strain 1.75 %,
Temperature 0.000 °C
399 ksi
@Strain 1.75 %,
Temperature 32.0 °F
 2.80 GPa
@Strain 1 %,
Temperature 0.000 °C
406 ksi
@Strain 1 %,
Temperature 32.0 °F
 3.00 GPa
@Strain 1.7 %,
Temperature -20.0 °C
435 ksi
@Strain 1.7 %,
Temperature -4.00 °F
 3.25 GPa
@Strain 0.0 %,
Temperature 0.000 °C
471 ksi
@Strain 0.0 %,
Temperature 32.0 °F
 4.00 GPa
@Strain 0.0 %,
Temperature -20.0 °C
580 ksi
@Strain 0.0 %,
Temperature -4.00 °F
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohm500V; IEC 60093
Comparative Tracking Index 600 V600 VSol. A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 11357-1/-3
Hot Ball Pressure Test >= 125 °C>= 257 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FISO 75/2Af
Vicat Softening Point 170 °C
@Load 5.10 kg
338 °F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Flame Spread <= 30.0 mm/min
@Thickness 3.00 mm
<= 1.18 in/min
@Thickness 0.118 in
Automotive Interior; ISO 3795
Glow Wire Ignition Temperature 675 °C
@Thickness 2.00 mm
1250 °F
@Thickness 0.0787 in
IEC 60695-2-13
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 70.0 - 80.0 °C158 - 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI119 / 313620

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.