MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® HHM 5502-04BN HDPE Hexene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergents. Meets ASTM D4976 - PE 235. ASTM D1248 - Type III, Class A, Category 5. FDA Regulation 177.1520, suitable for food packaging. Listed in drug master file.

Characteristics: excellent stiffness, exceptional stress crack resistance

Applications: bottles for bleach and detergent, industrial chemicals, industrial parts

Data provided by Chevron Phillips Chemical Company, LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³ASTM D1505
ESCR 100% Igepal® 35 hour35 hourCond. B; F50; ASTM D1693
 45 hour45 hourCond. A; CO-630; F50; ASTM D1693
 250 hour
@Temperature 60.0 °C
250 hour
@Temperature 140 °F
Bottle; F50; 10 ounce, 23-gram bottle, 10% fill, Joy Dishwashing liquid
High Load Melt Index 40 g/10 min
@Load 21.6 kg,
Temperature 190 °C
40 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.6 MPa4000 psiType IV; 50 mm per min; ASTM D638
Elongation at Break >= 600 %>= 600 %Type IV; 50 mm per min; ASTM D638
Flexural Modulus 1.38 GPa200 ksi0.5"/min crosshead speed; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -118 °C<= -180 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 171 - 182 °C340 - 360 °FThermoforming Surface Temp
 171 - 204 °C340 - 399 °FBlow Molding Stock
 194 - 216 °C381 - 421 °FExtrusion Stock

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer
Chevron Phillips Marlex® HHM 5502 LD High Density Ethylene Hexene Copolymer with Antistat
Chevron Phillips Marlex® HHM 5502-01 ST High Density Ethylene Hexene Copolymer
Chevron Phillips Marlex® HHM 5502-02 LD High Density Ethylene Hexene Copolymer with Antistat
Chevron Phillips HiD® 99416 with Food Grade Antistat HDPE Blow Molding Resin

PCHEVM39 / 20329

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.