MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil ESCOR™ AT 310 Extrusion Coating Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid; Ethylene Methyl Acrylate

Material Notes: ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable for use as a polymer modifier to improve bonding and toughness.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.941 g/ccExxonMobil Method
Methyl Acrylate Content 6.5 %
Acrylic Acid Content 6.5 %
Melt Flow 6.0 g/10 minASTM D1238
Neck In 3.50 cmat 200 m/min, 35 rpm, 295°C; ExxonMobil Method
 3.70 cmat 100 m/min, 35rpm, 295°C; ExxonMobil Method
Drawdown 770 ft/minat 35 rpm, 295°C; ExxonMobil Method
 970 ft/minat 65 rpm, 295°C; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 187 °FPeak Melting Temperature; ExxonMobil Method
Vicat Softening Point 142 °FASTM D1525
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
ExxonMobil ESCOR™ AT 310 Blown Film Resin
ExxonMobil ESCOR™ AT 310 Cast Film Resin
ExxonMobil ESCOR™ AT 310 Molding, extrusion and compounding resin
ExxonMobil ESCOR™ AT 320 Blown Film Resin

PEXB178 / 37483

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.