MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wellman Wellpet® PR109-N1 Unfilled PET  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Description: Unfilled PET

Information provided by Wellman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ISO 1183-87
Linear Mold Shrinkage 0.0010 - 0.0050 cm/cm0.0010 - 0.0050 in/inISO DIS 294-4
Melt Flow 3.5 g/10 min
@Load 0.325 kg,
Temperature 280 °C
3.5 g/10 min
@Load 0.716 lb,
Temperature 536 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7979ASTM D-2240
Tensile Strength at Break 60.0 MPa8700 psiISO 527-93
Elongation at Break 250 %250 %ISO 527-93
Flexural Strength 60.0 MPa8700 psiISO 178-93
Flexural Modulus 2.70 GPa392 ksiISO 178-93
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²ISO 180-93
 
Thermal PropertiesMetricEnglishComments
Melting Point 245 °C473 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FISO 75-93
 
Optical PropertiesMetricEnglishComments
Haze 10 %10 %ASTM D-2240
Transmission, Visible 87 %87 %ASTM D-1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Eastar GN071 Natural PETG Copolyester
Eastman Eastalloy DA510 Polymer
Aclo Acculoy POL063L Polycarbonate PET Alloy
Toyobo VYLOPET® EMC407 Non-Reinforced
Quantum PET

PWEL737 / 72453

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.