MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC NORYL™ Resin LTA6020 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ LTA6020 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2.5mm, 5VB at 2mm, and V0 at 1.5mm. NORYL LTA6020 exhibits good dimensional stability over a wide temperature range, high heat performance, low moisture uptake, and offers long-term aging / retention of mechanical properties. It is an excellent candidate for solar / photovoltaic (PV) junction boxes and outdoor electrical enclosures.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity  8.0 cP
@Load 5.00 kg,
Temperature 280 °C
8.0 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
 20 cP
@Load 5.00 kg,
Temperature 300 °C
20 cP
@Load 11.0 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 250 °C
4.0 g/10 min
@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 57.0 MPa8270 psi50 mm/min; ISO 527
Tensile Strength, Yield 71.0 MPa10300 psi50 mm/min; ISO 527
 72.0 MPa10400 psi50 mm/min; ASTM D638
Elongation at Break 8.0 %8.0 %50 mm/min; ISO 527
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527
 6.0 %6.0 %50 mm/min; ASTM D638
Tensile Modulus 2.68 GPa389 ksi1 mm/min; ISO 527
Flexural Strength 105 MPa15200 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
 105 MPa15200 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.58 GPa374 ksi2.6 mm/min, 100 mm span; ASTM D790
 2.60 GPa377 ksi2 mm/min; ISO 178
Izod Impact Notched 220 J162 ft-lbASTM D256
Izod Impact, Notched (ISO) 16.0 kJ/m²7.61 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -40.0 °C
3.81 ft-lb/in²
@Temperature -40.0 °F
80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -20.0 °C
4.76 ft-lb/in²
@Temperature -4.00 °F
80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature -10.0 °C
5.23 ft-lb/in²
@Temperature 14.0 °F
80*10*4; ISO 180/1A
 12.0 kJ/m²
@Temperature 0.000 °C
5.71 ft-lb/in²
@Temperature 32.0 °F
80*10*4; ISO 180/1A
Charpy Impact Unnotched 1.80 J/cm²8.57 ft-lb/in²ISO 179/2C
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 250 - 400 V250 - 400 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=1.00 mm
>= 120 sec
@Thickness >=0.0394 in
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=1.00 mm
60 - 120 arcs
@Thickness >=0.0394 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
 135 °C275 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °C277 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 123 °C253 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 126 °C
@Thickness 6.40 mm
259 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 144 °C291 °FRate B/120; ISO 306
 155 °C311 °FRate A/120; ISO 306
UL RTI, Electrical 125 °C257 °FUL 746B
UL RTI, Mechanical with Impact 125 °C257 °FUL 746B
UL RTI, Mechanical without Impact 125 °C257 °FUL 746B
Flammability, UL94  V-1
@Thickness >=1.00 mm
V-1
@Thickness >=0.0394 in
UL 94
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
 5VB
@Thickness >=2.00 mm
5VB
@Thickness >=0.0787 in
UL 94
 5VA
@Thickness >=2.50 mm
5VA
@Thickness >=0.0984 in
UL 94
Glow Wire Ignition Temperature  825 °C
@Thickness 1.00 mm
1520 °F
@Thickness 0.0394 in
IEC 60695-2-13
 825 °C
@Thickness 1.50 mm
1520 °F
@Thickness 0.0591 in
IEC 60695-2-13
 825 °C
@Thickness 2.00 mm
1520 °F
@Thickness 0.0787 in
IEC 60695-2-13
 825 °C
@Thickness 3.00 mm
1520 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-12
 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Zone 2 280 - 300 °C536 - 572 °F
Zone 3 270 - 290 °C518 - 554 °F
Melt Temperature 280 - 300 °C536 - 572 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 105 °C221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82347 / 290294

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.