MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Luflexen hyPE 52R FA HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Luflexen hyPE 52R FA is a high performance, high density polyethylene grade. This grade contains hexene as comonomer and offers good processability in a broad processing window. Luflexen hyPE 52R FA can be used in blown and cast films, textile and stretched applications. It contains antioxidants and is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications.

Availability: Europe

Application: Food Packaging Film; Lamination Film; Nets

Market: Flexible Packaging; Textile

Processing Method: Blown Film; Cast Film; Monofilament

Attribute: Antioxidant; Good Flow; High Stiffness; Low Gel

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccISO 1183-1
Melt Flow 2.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 1000 %ISO 527-1, -3
Film Elongation at Break, TD 1000 %ISO 527-1, -3
Elmendorf Tear Strength MD 65.0 gASTM D1922
Elmendorf Tear Strength TD 190 gASTM D1922
Film Tensile Strength at Break, MD 48.0 MPaISO 527-1, -3
Film Tensile Strength at Break, TD 46.0 MPaISO 527-1, -3
 
Thermal PropertiesOriginal ValueComments
Melting Point 131 °CPeak; ISO 11357-3
 
Optical PropertiesOriginal ValueComments
Haze <= 30.0 %ASTM D1003
Gloss >= 45.0 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9645 / 324580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.