MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polymer Industries Densetec HDPE Sheet
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Polymer Industry`s Densetec High Density Polyethylene sheet exhibits the properties of high impact strength, abrasion resistance, and low coefficient of friction. The material is also moisture, stain and odor resistant, and is FDA approved to be used in the food processing industry. The material`s durability makes it ideally suited for a variety of applications such as water tanks, chute linings and numerous industrial uses.

Information provided by Polymer Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D1505
ESCR 100% Igepal® 35 hourCO-630; Condition B; ASTM D1693
 45 hourCO-630; Condition A; ASTM D1693
Melt Index of Compound 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 28.0 MPa2in (50mm) per min.; ASTM D638 Type 4
Elongation at Break >= 600 %2in (50mm) per min.; ASTM D638 Type 4
Flexural Modulus 1.378 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µin/in-°F
@Temperature 20.0 °C
ASTM E831
Brittleness Temperature <= -84.0 °CASTM D746
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos T50-500 HDPE
Polymer Industries Densetec HDPE Pipe Grade
Polymer Industries Polyslick UHMW Sheet
Polymer Industries Polyslick UHMW Rod
Polymer Industries Densetec HMW Sheet

PPOLIND01 / 56977

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.