MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 699 X 144696 A Acrylonitrile Butadiene Styrene (ABS); ESD Protection - Permanently Static Dissipative - PTFE Lubricated - Extrusion Grade - Preliminary Datasheet
Categories: Polymer; Thermoplastic; ABS Polymer

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D 792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0080 in/in
@Thickness 0.126 in
ASTM D 955
Melt Flow <= 5.0 g/10 min
@Load 5.00 kg
<= 5.0 g/10 min
@Load 11.0 lb
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767instantaneous; ASTM D 2240
Tensile Strength at Break 26.9 MPa3900 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 1.38 GPa200 ksiASTM D 638
Flexural Strength 45.5 MPa6600 psiASTM D 790
Flexural Modulus 1.52 GPa220 ksiASTM D 790
Izod Impact, Notched 1.33 J/cm
@Thickness 3.20 mm
2.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 - 1.00e+9 ohm-cm1.00e+7 - 1.00e+9 ohm-cmASTM D 257
Surface Resistivity per Square 1.00e+8 - 1.00e+10 ohm1.00e+8 - 1.00e+10 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 238 °C400 - 460 °F
Drying Temperature 82.2 °C
@Time 7200 sec
180 °F
@Time 2.00 hour
Moisture Content 0.10 %0.10 %
Dew Point -17.8 °C0.000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LNP Lubricomp® AL-4010 HP GN4-678 Acrylonitrile Butadiene Styrene, PTFE Additive
LNP Lexan® SML6314 ABS + PC Alloy, 5% PTFE Lubricant
LNP CYCOLOY® DC8516 ABS + PC Alloy, 10.0 % PTFE Lubricant
LG Chemical SH610S ABS, Excellent Surface, High Impact
LG Chemical SH610A ABS, High Impact

PQZRA37515 / 205849

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.