MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dura-Bar 65-45-12 HRDS Continuously Cast Ductile Iron Bar Stock ASTM A536
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron; Ferritic

Material Notes: Dura-Bar 4512 HRDS is a high-silicon ductile iron intended for use at elevated temperatures or when a part is subjected to thermal cycling, such as permanent mold applications. The ferritic structure will remain stable so that no significant transformation takes place, thereby minimizing stresses that lead to cracks and distortion of the finished part.

The microstructure will contain Type I and II nodules as defined in ASTM A247. The matrix will be predominantly ferrite with some pearlite. Chill carbides will be less than 5% in any field at 100x and will be well dispersed.

4512 HRDS is not intended for hardening. The matrix structure may be softened slightly by heating to 1400F (760C) and furnace cooling to 400F (205C).

4512 HRDS is most commonly used in high temperature applications where resistance to growth and oxidation is required.

Composition: Typical chemical composition and ranges, actual values depend on cross section size.

Information provided by Dura-Bar.

Key Words: high-silicon ductile iron, high strength cast iron, 4512
Vendors: Dura-Bar Metal Services is the leading supplier of Dura-Bar® continuous cast iron and a major distributor of bronze alloys. Our customers rely on us for high quality materials that help increase their profitability. Call us at 1-800-526-0548 or visit dura-barms.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 167 - 229167 - 229Depends on cast section size and location of test
Tensile Strength, Ultimate 448 MPa65000 psi
 37.9 MPa
@Temperature 788 °C
5500 psi
@Temperature 1450 °F
 68.9 MPa
@Temperature 704 °C
10000 psi
@Temperature 1300 °F
 186 MPa
@Temperature 593 °C
27000 psi
@Temperature 1100 °F
 359 MPa
@Temperature 482 °C
52000 psi
@Temperature 900 °F
Tensile Strength, Yield 310 MPa45000 psi
 31.0 MPa
@Temperature 788 °C
4500 psi
@Temperature 1450 °F
 51.7 MPa
@Temperature 704 °C
7500 psi
@Temperature 1300 °F
 159 MPa
@Temperature 593 °C
23000 psi
@Temperature 1100 °F
 324 MPa
@Temperature 482 °C
47000 psi
@Temperature 900 °F
Elongation at Yield 12 %12 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.45 - 3.75 %3.45 - 3.75 %
Iron, Fe 92.1 - 93 %92.1 - 93 %As Balance
Manganese, Mn 0.15 - 0.35 %0.15 - 0.35 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si 3.45 - 3.75 %3.45 - 3.75 %
Sulfur, S <= 0.02500 %<= 0.02500 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536
Ductile Iron grade 65-45-12
Dura-Bar 80-55-06 Continuously Cast Ductile Iron Bar Stock ASTM A536
Dura-Bar G1 Continuously Cast Gray Iron Bar Stock ASTM A48
Dura-Bar G2A Continuously Cast Gray Iron Bar Stock ASTM A48

NDURA04A / 138289

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.