MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Visico™ LE0540 Polyethylene Semiconductive Compound, Crosslinkable  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Visico™ LE0540 is a silane crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Visico™ LE0540 is highly suitable for co-extrusion with LDPE silane crosslinkable insulation materials. Applications: Visico™ LE0540 is intended for semiconductive applications for silane crosslinkable medium voltage cables with rated voltages up to 36 kV. Specifications: AEIC CS8; BS 6622; Cenelec HD 620 S-1; IEC 60502; ISO 1872-E/BA, KHXY, 23-G200, C30; and NF C33-223.

Information provided by Borealis AG

Key Words: XLPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183/ISO 1872-2
Water Absorption 0.020 %0.020 %Karl Fischer-titration
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50501s; ISO 868
Tensile Strength at Break <= 2.60 MPa<= 377 psiafter aging (240h, 135°C); IEC 60811-1-2
 >= 13.0 MPa>= 1890 psi25mm/min; ISO 527
Elongation at Break 400 %400 %25mm/min; ISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  <= 100 ohm-cm
@Temperature 23.0 °C
<= 100 ohm-cm
@Temperature 73.4 °F
ISO 3915
 <= 1000 ohm-cm
@Temperature 90.0 °C
<= 1000 ohm-cm
@Temperature 194 °F
ISO 3915
 
Processing PropertiesMetricEnglishComments
Zone 2 150 °C302 °F
Zone 3 150 °C302 °F
Zone 4 150 °C302 °F
Melt Temperature 170 °C338 °F
Head Temperature 150 °C302 °F
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
High Temperature Pressure Test, %< 590°C, 6h; IEC 60811-3-1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Visico™/Visico™ LE4421M/LE4431M Polyethylene
Borealis FL5580 High Density Polyethylene
Avient Syncure™ System S112NA Polyethylene, Crosslinked (XLPE)
Borealis Borlink™ LE0594 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Borealis Borlink™ LE0595 Crosslinkable Semiconductive Compound for Shielding of Power Cables

PBOREA599 / 108858

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.