MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese SO.F.TER Sofprene T® 5420.A90 SBS TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Injection molding, high fluidity grade

Sofprene T® is a thermoplastic elastomer with SBS. Applications include Furniture (shock-absorbers for bed slats, wheels, anti-shocks profiles), Household goods (anti-slip mats, handles for tools, overmolded rubber lips for dustpan and squeegees, plungers), and Toys (wheels, handles, seats, little toys).

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D2240
Tensile Strength 9.00 MPa1310 psiASTM D412 C
Elongation at Break 650 %650 %ASTM D412-C
100% Modulus 4.80 MPa
@Strain 100 %
696 psi
@Strain 100 %
ASTM D412 C
Tear Strength 44.0 kN/m251 pliASTM D624 C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 5430 Low Density Polyethylene, Cast Film
Ineos Nova 5420 High Impact Polystyrene
3M 5430 Squeak Reduction Tape
SIDPEC EGYPTENE® HD 5420 GA HDPE Blow Molding
Henkel Loctite® 5420 Heat Cure Form-In-Place Electrically Conductive Silicone Sealant

PSOFS762 / 162226

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.