VECTOR® 4411AS is a linear triblock copolymer with narrow molecular weight distributions. The product exhibits the following characteristics: - High styrene content, high modulus, low viscosity and excellent creep resistance.
- Well-suited for use in hot melt adhesives for hygiene and compatibilization of styrenic/olefinic polymer blends.
Information provided by TSRC Corporation |