Description: This is a water repellent, non-melting silicone grease developed to meet the special requirement of High Voltage insulator coating Key Features - Excellent work stability
- Non melting even in hot climates
- Tinted pink for visual inspection aid
- Excellent water repellence
Key Applications Application: Humidity and industrial/natural contaminants have long been a cause of leakages and flashovers on HV insulators. Experience has shown that a layer of silicone grease can eliminate this problem, not only by shedding water, but also by encapsulating any contaminating particles, thus preserving an unbroken dielectric surface at all times.Information provided by CHT Group |