MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Resirene Resiprene® 1075 170P Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Resiprene® 1075 170P is a Thermoplastic Elastomer (TPE) easy to process and great for injection molding process. Features: Easy color match, excellent process ability, Good Mechanical Properties, 100% recyclable, Process with thermoplastics traditional equipment, No predrying.

Applications: Tools handles, pipes, impact modifier, tooth brush handles, seals, soft touch applications.

Information provided by Resirene

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7676DIN 53505
Hardness, Shore D 2323DIN 53505
Tensile Strength at Break 5.09 MPa738 psiASTM D638
Elongation at Break 1100 %1100 %ASTM D638
100% Modulus 0.910 MPa
@Strain 100 %
132 psi
@Strain 100 %
ASTM D638
200% Modulus 1.13 MPa
@Strain 200 %
164 psi
@Strain 200 %
ASTM D638
300% Modulus 1.32 MPa
@Strain 300 %
191 psi
@Strain 300 %
ASTM D638
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 280 °C<= 536 °F
Rear Barrel Temperature 160 - 170 °C320 - 338 °F
Middle Barrel Temperature 170 - 180 °C338 - 356 °F
Front Barrel Temperature 180 - 190 °C356 - 374 °F
Nozzle Temperature 200 - 210 °C392 - 410 °F
Mold Temperature <= 45.0 °C<= 113 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESIR917 / 250138

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.