MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt EASY FLO 30 Silver Based Cadmium-Bearing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes:

Applications: Easy-Flo 30 is a are good general purpose, low temperature silver brazing filler metals for joining both ferrous and nonferrous metals. Because of their fairly low cost, good fatigue strength and ability to make leak-tight joints where close clearances cannot be maintained, they have been widely used in the refrigeration and air-conditioning industry. Additional uses for these filler metals are tubular bicycle and furniture frames, where joint fitup may be variable.

Characteristics: Easy-Flo 30 is a low temperature, economical, brazing filler metals capable of bridging gaps where poor joint fitup cannot be avoided. This filler metal has a tendency to liquate (i.e., separate into low and high melting constituents) when heated slowly and therefore it is preferable to use them where the heat source is sufficient to raise the part temperature rapidly through the melting range of the brazing filler meta. Handy Flux is recommended for use with this filler metal.

Specifications:This filler metal conform to the following specifications: AWS A5.8 BAg-2a, ASME Boiler and Pressure Vessel Code Section II-C SFA 5.8 BAg-2a

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.09 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000518 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 1125 - 1310 °F
Solidus 1125 °FMelting Point
Liquidus 1310 °FFlow Point
Maximum Service Temperature, Air 400 °Fcontinuous
 600 °Fintermittent
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd 19 - 21 %
Copper, Cu 26 - 28 %
Other, total <= 0.15 %
Silver, Ag 29 - 31 %
Zinc, Zn 21 - 25 %
 
Descriptive Properties
ColorLight Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Superplastic Zinc (Zn-22Al), As-Rolled - Longitudinal Properties
Seashell Technology Silver Nanowires
Sandvik Cuprothal 5 Resistance Wire
Materion C118 Electrical Contact Alloy
Lord Adhesives Thermoset™ MD-150 Conductive Adhesive

NLUCMI46 / 18113

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.