PC0798 is a flame retardant crosslinking polyethylene compound for low voltage insulation. PC0798 is a halogenated, colorable, chemically crosslinkable copolymer compound which contains flame retardant additives to reduce normal flame spread characteristics so as to achieve a flame resistant rating when used according to the UL 44 Horizontal test on 14 AWG. Specifications Underwriters Laboratories Standards 44 and 854.Information provided by Borealis AG |