Polypropylene Homopolymer, Excellent Long Term Heat and Color StabilityApplications- Coolant bottle reservoirs
- Overflow tanks
- Blow molded parts
Molding Temperatures- Rear Temperature: 145-200°C
- Middle Temperature: 210-235°C
- Front and Nozzle Temps: 210-235°C
- Stock Temperature: 227-260°C
- Mold Temperature: 23-50°C
Processing conditions- Suggested shot size: 50-70%
- First stage injection pressure: Maximize
- Screw Speed: 30-60%
- Packing pressure: Minimize
- Back Pressure: 50-150 psi
Other molding considerations: Melt temperature above 260°C may cause resin degradation and changes to resin properties. To improve dispersion of color concentrates use a screw with a mixing zone or mixing nozzle. Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued prior to the shutdown announcement. |
Information Provided by Chevron Phillips Chemical |