MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sumitomo Bakelite POROPHEN® GF 9200 L12 Phenolic Molding Compound
Categories: Polymer; Thermoset; Phenolic

Material Notes: POROPHEN® GF 9200 L12 is a long glass fiber reinforced phenolic molding compound with high mechanical strength and excellent thermal properties.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.79 g/cc0.0647 lb/in³ISO 1183
Water Absorption 0.40 %0.40 %ISO 62
Linear Mold Shrinkage 0.00080 cm/cm0.00080 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 160 MPa23200 psiISO 527-1
Tensile Modulus 26.0 GPa3770 ksiISO 527-1
Flexural Strength 356 MPa51600 psiISO 178
Flexural Modulus 23.0 GPa3340 ksiISO 178
Flexural Strain at Break 0.64 %0.64 %ISO 178
Compressive Strength 387 MPa56100 psiISO 604
Charpy Impact, Notched 6.00 J/cm²28.6 ft-lb/in²ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 150 V150 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C5.56 µin/in-°FTMA
CTE, linear, Transverse to Flow 22.0 µm/m-°C12.2 µin/in-°FTMA
Shrinkage -0.0200 %-0.0200 %Post; ISO 2577

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite POROPHEN® GF 9202 L12 Phenolic Molding Compound
Ineos L12Z-01 Polypropylene Impact Copolymer

PSUMIT190 / 193995

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.