MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Akulon® F132-E2 PA6, High Viscosity, Nucleated, Lubricated, Film Extrusion
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Film Grade; Nylon 6, Nucleated

Material Notes: High Viscosity, Nucleated, Lubricated, Film Extrusion

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Water Vapor Transmission 35.0 g/m²/dayDIS 15106-1/-3
Oxygen Transmission 1.00 cc-mm/m²-24hr-atm0% RH; DIS 15105-1/-2
 1.55 cc-mm/m²-24hr-atm85% RH; DIS 15105-1/-2
Viscosity 1120 cP
@Temperature 260 °C
Melt; DSM Method
 50 cP
@Shear Rate 10000 1/s,
Temperature 280 °C
 50 cP
@Shear Rate 10000 1/s,
Temperature 260 °C
 50 cP
@Shear Rate 10000 1/s,
Temperature 240 °C
 500 cP
@Shear Rate 100 1/s,
Temperature 280 °C
 600 cP
@Shear Rate 0.1 1/s,
Temperature 280 °C
 700 cP
@Shear Rate 100 1/s,
Temperature 260 °C
 1000 cP
@Shear Rate 100 1/s,
Temperature 240 °C
 1000 cP
@Shear Rate 0.1 1/s,
Temperature 260 °C
 2500 cP
@Shear Rate 0.1 1/s,
Temperature 240 °C
Viscosity Number 210 cm³/gISO 307, 1157, 1628
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 34.0 MPaISO 527-3
Film Elongation at Break, MD 350 %ISO 527-3
Modulus of Elasticity 0.465 GPa50 mm/min; DSM Method
Coefficient of Friction, Dynamic 0.80ISO 8295
Coefficient of Friction, Static 1.4ISO 8295
Tear Strength Test 32Trouser Tear resistance, parallel; ISO 6383-1
Film Tensile Strength at Break, MD 96.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°CISO 11359-1/-2
Specific Heat Capacity 1.55 J/g-°C
 2.25 J/g-°C
@Temperature 20.0 - 150 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 85 %DSM Method
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 °CExtruder
Die Temperature 270 °C
Roll Temperature 110 °CChill
 
Descriptive Properties
Puncture resistance1230 J/mDSM Method
RSV formic acid3.2[1g/100ml], DSM Method
Type of extrusionCast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B36 LN 01 PA6
Envalior Akulon® F130-E1 PA6, Medium Viscosity, Nucleated, Lubricated, Film Extrusion
DuPont Mobility and Materials Zytel® ST801 BK010A PA66-HI
Envalior Akulon® K224-G6 PA6-GF30, Dry, 30% Glass Filled
Envalior Akulon® K222-DL PA6, Dry, Low Viscosity, Heat Stabilized, Light Stabilized

PDSM8008 / 184709

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.