MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Marex Composites Mycell M130 PVC Foam Core
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: Mycell is a PVC structural foam material that Marex Composites customizes for standard finishes from Maricell in Italy.

Property data reported are nominal/average values.

Information provided by Marex Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.130 g/cc0.00470 lb/in³ISO 845
Water Absorption 1.0 %1.0 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 4.20 MPa609 psiASTM D1623
Elongation at Break 45 %45 %Shear elongation; ISO 1922
Tensile Modulus 0.155 GPa22.5 ksiASTM D1623
Compressive Strength 3.07 MPa445 psiISO 844
Compressive Modulus 0.162 GPa23.5 ksiISO 844
Shear Modulus 0.0480 GPa6.96 ksiASTM C393
Shear Strength 2.57 MPa373 psiASTM C393
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0390 W/m-K0.271 BTU-in/hr-ft²-°FISO 8301
 
Descriptive Properties
ColorBlue
Fire ResistanceDIN5510 S4 SR2 ST2 FED<1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMAREX975 / 230571

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.