MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos H38G-02 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade; Polypropylene, Molded

Material Notes: This is a polypropylene homopolymer for general purpose injection molding and high speed spinning applications. It is useful for spun bonded nonwovens and partially oriented yarn (POY). This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

    Applications
  • Fiber and tape
  • General purpose injection molding
  • Nonwoven fabrics
  • Partially oriented yarn
  • Staple fiber

    Benefits
  • Excellent gas fade resistance
  • Excellent processability
  • High line speeds
  • Narrow molecular weight distribution

Information provided by Ineos Olefins & Polymers USA

Key Words: General purpose
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.909 g/cc0.0328 lb/in³ASTM D792
Melt Flow 38 g/10 min
@Load 2.16 kg,
Temperature 230 °C
38 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100100ASTM D785
Tensile Strength at Break 17.8 MPa2580 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 33.6 MPa4870 psi2.0 in/min; ASTM D638
Elongation at Break 530 %530 %2.0 in/min; ASTM D638
Elongation at Yield 11 %11 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1300 MPa189000 psiASTM D790A
Izod Impact, Notched 0.240 J/cm0.450 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 2.37 kJ/m²1.13 ft-lb/in²Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C195 °FUnannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 69.2 %
@Thickness 1.27 mm
69.2 %
@Thickness 0.0500 in
ASTM D1003
Gloss 93 %93 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ProcessFiber
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos H12G-01 Polypropylene Homopolymer
Ineos H36G-01 Polypropylene Homopolymer
Ineos N12N-00 Polypropylene Impact Copolymer
Ineos R35C-01 Polypropylene Random Copolymer
Ineos R35C-02 Polypropylene Random Copolymer

PINEOS051 / 99372

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.