MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon 55133R062 0.0622" (1.58 mm) Cured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
Interleave: Polyethylene
Side 1: Cured Silicone Rubber
Substrate: Style 162 Fiberglass
Side 2: Cured Silicone Rubber

Product Use: Press Pad

Appearance: Red silicone rubber on fiberglass cloth

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 74.9 microns2.95 milInterleave
 480 microns18.9 milSubstrate; Arlon SQA-TMS-003
 551 microns21.7 milSide 1; Arlon SQA-TMS-003
 551 microns21.7 milSide 2; Arlon SQA-TMS-003
 1580 microns62.2 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050Silicone Property; ASTM D2240
 7070Product Property; ASTM D2240
Tensile Strength 8.20 MPa1190 psiSilicone Property; ASTM D412
Elongation at Break 765 %765 %Silicone Property; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 300 °C572 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month
@Temperature 23.0 °C
60.0 Month
@Temperature 73.4 °F
From date of manufacture
 
Descriptive Properties
ColorNaturally WhiteSubstrate
 Red
Recommended Application Pressure0 - 5 Mpa
Service Life(200°C and 2.07MPa)
 (225°C and 2.07MPa)
 (250°C and 2.07MPa)
Total Product Weight (g/m2)1638Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon CP-510R Silicone Rubber
Rogers Arlon CP-427R Silicone Rubber
Rogers Arlon CP-414R Silicone Rubber
Rogers Arlon CP-375CR Silicone Rubber
Rogers Arlon 99202R008 0.008" (0.203 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Carrier

PARL341 / 125527

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.