MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wacker Belsil® DM 1000 Dimethicone
Categories: Fluid; Polymer

Material Notes: BELSIL® DM 1000 is a linear, non-reactive, unmodified polydimethylsiloxane. BELSIL® DM 1000 is characterized by low surface tension and a high spreading coefficient. Due to their flexible polymer backbone, dimethicones have high permeability to gases (e.g. water vapor, oxygen), which allows respiration of the skin.

Application: BELSIL® DM 1000 is used in a broad range of personal care formulations as an emollient. It allows formulators to adjust spreadability and conditioning effects. Whitening and stickiness of cosmetic products can be reduced and skin feel can be optimized.

INCI name: Dimethicone

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccDIN 51757
Viscosity 1000 cPdynamic; DIN 53019
Kinematic Viscosity 1000 cStDIN 53019
Surface Tension 0.021 dynes/cm
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 300 °CISO 2592
Ignition Temperature 410 °CEN 14522
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4035
Transmission, Visible 90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Aggregate stateliquid
Appearancecolorless, clear
SolubilityBELSIL® DM 1 Plus>10%
 BELSIL® DM 10>10%
 BELSIL® DM 12500>10%
 BELSIL® DM 350>10%
 BELSIL® DM 60000>10%
 C12-15 alkyl benzoatesinsoluble
 C9-13 isoparaffin>10%
 Castor oilinsoluble
 Cyclopentasiloxane>10%
 Ethanolinsoluble
 Ethyl acetate>10%
 Glycerininsoluble
 Isopropanolinsoluble
 Isopropyl myristate>10%
 Lanolin oilinsoluble
 Mineral oil (high-viscosity)insoluble
 Mineral oil (low-viscosity)insoluble
 Octyldodecanolinsoluble
 Oleyl oleateinsoluble
 Olive oilinsoluble
 Propylene glycolinsoluble
 Waterinsoluble
 Wheat germ oilinsoluble

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9020 / 204549

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.