0.010 in. (0.25 mm) minimum uncured silicone on 0.002 in. (0.5 mm) minimum cured silicone on 0.008 in. (0.2 mm) nominal Prime Coated 7628 Fiberglass; 0.0015 in. (0.038 mm) polyethylene interleave; overall thickness 0.020 in ± 0.001 (0.51 mm ± 0.03). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 627.3 g/m² ± 67.8 (18.5 oz./yd.² ± 2.0). Shelf Life: 6 months from date of manufacture at 23.8°C (75°F). Cure Time: 0.25 hours. Post Cure: 204°C (400°F), for 2 hours. Information provided by the manufacturer, Arlon Silicone Technologies Division. Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation. |