MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

VICTREX™ PEEK FG™ 700 Food Grade PEEK, High Strength
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for composite manufacture, easy flow, FDA food contact compliant, color natural. Applications for higher strength in a static system. Low coefficient of thermal expansion. Chemically resistant to aggressive environments, suitable for sterilization for medical and food contact applications.

Information Provided by Victrex.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.300 g/cc0.0108 lb/in³ISO 1183
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Particle Size 10 µm10 µmD50; ISO 13320-1
Viscosity 130 cP
@Temperature 400 °C
130 cP
@Temperature 752 °F
Melt; ISO 11443
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psiISO 527-2
Elongation at Break 15 %15 %ISO 527-2
Tensile Modulus 4.10 GPa595 ksiISO 527-2
Flexural Modulus 3.90 GPa566 ksiISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²2.14 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) NBNBISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 343 °C649 °FISO 11357-3
Glass Transition Temp, Tg 143 °C289 °FOnset; ISO 11357-2
 147 °C297 °FMidpoint; ISO 11357-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 380 - 400 °C716 - 752 °F
Drying Temperature 120 - 150 °C
@Time 10800 - 18000 sec
248 - 302 °F
@Time 3.00 - 5.00 hour
Option 2
Moisture Content <= 0.020 %<= 0.020 %
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVICTB892a / 320026

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.