MARPOL® LDC 740 is a low density polyethylene resin recommended for use in the boardstock coating. This material has an excellent combination of low neck-in, ease of processing and good chill-roll release. Recommended application: Milk cartons, liquid containers, multiwall bag stock and frozen food containers, extrusion lamination, coextrusion coating, industrial packaging. Additives: Antiblock - no, slip - no. Information provided by Marco Polo International, LLC |