MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Permabond ET5401 Epoxy Resin
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and composites. Permabond ET5401 forms tough bonds providing high peel resistance and high shear strength coupled with excellent resistance to high temperatures. ET5401 performance is enhanced by curing at high temperature or being exposed to high temperature (such as during paint-stoving).

Features & Benefits:

  • Adhesion to a wide variety of substrates
  • Full cure at room temperature
  • Easy to apply
  • High shear and peel strength
  • Good impact strength
  • High temperature resistance
  • Non-drip rheology

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature 5.00 - 25.0 °C41.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 65 - 7565 - 75Cured at 25°C
 75 - 8575 - 85Cured for 1 hr at 80°C
Adhesive Bond Strength 6.00 - 8.00 MPa870 - 1160 psiFRP Glass Polyester, Shear; ISO 4587
 10.0 - 15.0 MPa1450 - 2180 psiGrit blasted mild steel, Shear; ISO 4587
 19.0 - 23.0 MPa2760 - 3340 psiFRP Glass Epoxy, Shear; ISO 4587
 22.0 - 24.0 MPa3190 - 3480 psiCarbon Fiber, Shear; ISO 4587
 20.0 - 30.0 MPa2900 - 4350 psiMild steel, Shear; ISO 4587
Peel Strength 5.60 - 6.40 kN/m32.0 - 36.5 pliCured for 1 hr at 80°C
 10.0 - 12.0 kN/m57.1 - 68.5 pliCured for 15 mins at 200°C
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 80.0 °C
1.00 hour
@Temperature 176 °F
full cure
 180 - 240 min
@Temperature 25.0 °C
3.00 - 4.00 hour
@Temperature 77.0 °F
handling time
 5760 - 10100 min
@Temperature 25.0 °C
96.0 - 168 hour
@Temperature 77.0 °F
full cure
Pot Life 10.0 - 12.0 min
@Temperature 25.0 °C
10.0 - 12.0 min
@Temperature 77.0 °F
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceBlack for Polyamine Hardener
 White for Epoxy Resin
Maximum Gap Fill (mm)5
Strength Retention100% at 0°CRelative to 0°C
 15% at 150°CRelative to 0°C
 80% at 100°CRelative to 0°C
 90% at 50°CRelative to 0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® F593 Epoxy Resin
Saint-Gobain Quartzel® Fiber/Epoxy Resin Unidirectional Composite
Röchling Glastic® EPC 308 Reinforced Epoxy Resin
Permabond ET500 Epoxy Resin
Master Bond EP21SC-1 Two Component Epoxy Resin System

PPERMA907 / 162776

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.