MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Haysite 14200 Polyester BMC, 15% Glass Reinforced
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: This grade can be compression, transfer, or injection molded. Good mechanical strength and exceptional arc/track properties make this grade a natural for many electrical applications. The 14200 BMC is recognized by UL with a 94V-0 flame rating at 0.120" wall thickness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.85 g/cc0.0668 lb/in³ASTM D572
Water Absorption 0.16 %0.16 %ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 41.0 MPa5950 psi
Flexural Strength 138 MPa20000 psi
Compressive Strength 97.0 MPa14100 psi
Izod Impact, Notched 4.30 J/cm8.06 ft-lb/inedgewise; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.0 kV/mm406 kV/inPerpendicular (ASTM D149), Short Time
Arc Resistance 194 sec194 secASTM D495
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °Ftemperature rating
Flammability, UL94 V-0V-0File No.E-27875

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHAY01 / 45607

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.