Hostacom TKC717D 8N84 MANDEL BEIGE medium melt flow, 2,200 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffness, impact resistance and processability. It is typically used for automotive interior applications that require high durability. Applications: Interior Automotive ApplicationsInformation provided by LyondellBasell. |