MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
AISI Type 302Cu Stainless Steel Annealed Sheet and Strip
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: Austenitic, exhibits lower rate of work than Type 305, non-magnetic in the annealed condition and becomes only very faintly magnetic after severe cold working, exhibits the same corrosion resistance as Type 304, subject to intergranular carbide precipitation when exposed to temperature ranges of 480-870°C, has a safe scaling temperature in continuous exposure of 870°C. Typical applications include cold formed nits and recessed head fasteners.

Key Words: UNS S30430
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 80
Tensile Strength, Ultimate 580 MPa
Tensile Strength, Yield 290 MPa
Elongation at Break 0.55 %
Modulus of Elasticity 193 GPa
Izod Impact 150 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000720 ohm-cm
Magnetic Permeability 1.02Approximate Value
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.3 µm/m-°C
@Temperature 0.000 - 100 °C
 17.8 µm/m-°C
@Temperature 0.000 - 315 °C
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.502 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.3 W/m-K
@Temperature 100 °C
 21.5 W/m-K
@Temperature 500 °C
Melting Point 1400 - 1450 °C
Solidus 1400 °C
Liquidus 1450 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 18 %
Copper, Cu 4.0 %
Iron, Fe 66 %
Manganese, Mn <= 2.0 %
Nickel, Ni 9.0 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
305 Stainless Steel, annealed, sheet
Type 304N High-Nitrogen Austenitic Stainless Steel, Annealed Bar, UNS S30451
AISI Type 304L Stainless Steel
308 Stainless steel, annealed, sheet and strip
AISI 302Cu Stainless Steel soft tempered 2.54- 25.4 mm diameter wire

MQM304A / 13805

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.