MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering S80U Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Translucent Silicone Rubber, 70 -80 °IRHD. Shore A Platinum cured Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Silicone compound in conformity with the requirements of USP 25, NF20, 2002, Class 6. Formulated using only those ingredients authorized by FDA CFR21 Section 177.2600. BGV XV compliant. Formulated to BS2494 Type ‘W’ and Water Research Council (WRC) tested in accordance with BS6920 ‘Items which have passed full tests of effects on water quality’ (for use in potable water applications). WRC approval No. 0005509. Tested to 3A requirements.

Applications: Compared to equivalent silicones, excellent mechanical and physical properties, and chemical stability over the temperature range of -60ºC to +200ºC. Excellent behaviour when sterilised. High transparency grade, intended for food contact, pharmaceutical contact, pharmaceutical and biomedical applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 78°IRHD; ASTM D1415
 83°IRHD, +5 change after 168 hours @ 200°C; ASTM D1415
Tensile Strength, Yield 8.50 MPaASTM D412
 9.35 MPa10% change after 168 hours @ 200°C; ASTM D412
Elongation at Break 472.8 %-1.5% change after 168 hours @ 200°C; ASTM D412
 480 %ASTM D412
Compression Set 32.2 %
@Temperature 175 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -60.0 °C
Flash Point >= 300 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CPT C-Flex® R70-085 Clear Biocompatible TPE
CPT C-Flex® R70-190 Opaque Biocompatible TPE
Fujipoly Industries Sarcon® 45H Thin-Film HR
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane
Dow HV 1760/80 SILICONE RUBBER NATURAL

PPRECI286 / 58010

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.