MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 538XT V30 Natural W PA6, 30% glass filled, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: Polyamide 6 reinforced with 30% of glass fibers, heat stabilized, with high viscosity and high toughness, for extrusion.

Available in: North America

Product Applications: This product is designed specifically for extrusion to be used in window profile and thermal break applications. This material is available in natural.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 142 MPaISO 527 Type 1A
Elongation at Break 142 %ISO 527 Type 1A
Tensile Modulus 8900 MPaISO 527 Type 1A
Flexural Strength 221 MPaISO 178
Flexural Modulus 6626 MPaISO 178
Izod Impact, Notched (ISO) 24.98 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 92.8 kJ/m²ISO 179/1eU
 
Processing PropertiesOriginal ValueComments
Feed Temperature 240 - 260 °C
Front Barrel Temperature 240 - 280 °C
 
Descriptive Properties
Compression Zone240-270°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® K224-PG8 PA6-I-GF40, Dry, 40% Glass Reinforced, Impact Modified
Domo TECHNYL® C 246SI V30 PA6, 30% glass filled, Conditioned
Domo TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY
Celanese Zytel® 80G14AHS BK099 PA66-IGF14
Celanese Zytel® 80G14A NC010A PA66-IGF14

PRHOD816 / 138047

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.