System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
AISI 5135H Steel
Categories:
Metal
;
Ferrous Metal
;
Alloy Steel
;
AISI 5000 Series Steel
;
Low Alloy Steel
;
Carbon Steel
;
Medium Carbon Steel
Key Words:
AFNOR 42 C 4 (Fr), ISO 683/VII 2a, ISO 683/VII 2b, ISO R683-7 2a, ISO R683-7 2b, B.S. 530 A 36, B.S. 530 H 36, B.S. Type 3, JIS SCr 3 H (Japan.), UNI 41 Cr 4 KB, UNS H51350, ASTM A304, SAE J1268, DIN 1.7035, AFNOR 42 C 4 (Fr), UNI 41 Cr 4 KB (Ital.)
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
7.85
g/cc
Mechanical Properties
Original Value
Comments
Hardness, Brinell
179 - 217
annealed and cold drawn.
Hardness, Knoop
220
Converted from Brinell
Hardness, Rockwell B
92
Converted from Brinell
Hardness, Rockwell C
13
Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers
208
Converted from Brinell
Modulus of Elasticity
205
GPa
Typical for steel
Bulk Modulus
160
GPa
Typical for steel.
Poissons Ratio
0.29
Calculated
Machinability
70 %
annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus
80.0
GPa
Typical for steel.
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.0000228
ohm-cm
@Temperature 20.0 °C
0.0000281
ohm-cm
@Temperature 100 °C
0.0000352
ohm-cm
@Temperature 200 °C
0.0000530
ohm-cm
@Temperature 400 °C
Thermal Properties
Original Value
Comments
Specific Heat Capacity
0.494
J/g-°C
Thermal Conductivity
46.6
W/m-K
Typical steel
Component Elements Properties
Original Value
Comments
Carbon, C
0.32 - 0.38 %
Chromium, Cr
0.70 - 1.15 %
Iron, Fe
97.495 - 98.33 %
As remainder
Manganese, Mn
0.50 - 0.60 %
Phosphorus, P
<= 0.035 %
Silicon, Si
0.15 - 0.30 %
Sulfur, S
<= 0.040 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
AISI 5132H Steel
AISI 5135 Steel
AISI 5132 Steel
AISI 5140 Steel, annealed 830°C (1525°F)
AISI 4137H Steel
M513CB / 8064
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.