MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parker Chomerics CHO-SEAL® 0860 Conductive Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.

Extruded only

RoHS Compliant

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 - 1.58 g/cc0.980 - 1.58 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 65 - 7565 - 75ASTM D2240
Tensile Strength >= 3.45 MPa>= 500 psiASTM D412
Elongation at Break >= 75 %>= 75 %ASTM D412
Tear Strength <= 8.77 kN/m<= 50.0 pliASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 3.0 ohm-cm<= 3.0 ohm-cmwithout pressure-sensitive adhesive; CEPS-0002
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °F
Minimum Service Temperature, Air -51.0 °C-59.8 °FFlex TR10
Flammability, UL94 HBHB
 
Descriptive Properties
BinderSilicone
FillerCarbon

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME222 / 130932

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.