MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Dow™ DMDA-8950 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow DMDA-8950 NT 7 HDPE is produced via UNIPOL™ Process Technology from Dow and is intended for use in thin-wall injection molding applications such as food containers. This resin has been designed to provide a good toughens and excellent processability.
Main Characteristics:
  • Injection molding
  • For injection molded thin-wall food
  • Excellent processability
  • Very narrow molecular weight distribution
Complies with: US FDA 21 CFR 177.1520©3.1a; Canadian HPFB No Objection; EU No 10/2011; US FDA DMF; US FDA 21 CFR 177.1520©3.2a. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©3.1a; Canadian HPFB No Objection; EU No 10/2011; DMF; FDA 21 CFR 177.1520©3.2a

Form: Pellets

Processing Method: Injection Molding

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ASTM D792
Melt Flow 66 g/10 min
@Load 2.16 kg,
Temperature 190 °C
66 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5959ASTM D2240
Tensile Strength at Break 28.3 MPa4100 psiASTM D638
Tensile Strength, Yield 17.2 MPa2500 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Elongation at Yield 1.0 %1.0 %ASTM D638
Flexural Modulus 1.00 GPa145 ksi2% Secant; ASTM D790B
Tensile Impact Strength 63.0 kJ/m²30.0 ft-lb/in²Type S; ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 128 °C262 °F
Crystallization Temperature 116 °C241 °F
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C156 °FUnannealed; ASTM D648
Vicat Softening Point 122 °C252 °FASTM D1525
Brittleness Temperature -75.0 °C-103 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF455 / 311148

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.