MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Nouryon Ethomeen O/12LC EMEIA Oleyl amine ethoxylate
Categories: Other Engineering Material

Material Notes: Ethomeen O/12LC is a tertiary amine ethoxylate, based on a primary oleyl amine.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³
Viscosity 150 cP150 cP
Surface Tension 28 dynes/cm28 dynes/cmaccording to Du Noüy, 25°C, 0.1%; DIN 53914
 
Thermal PropertiesMetricEnglishComments
Pour Point 1.00 °C33.8 °F
Flash Point >= 200 °C>= 392 °FPensky Martens Closed Cup
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 1.0 %<= 1.0 %
 
Descriptive Properties
AppearanceLiquid
Clear point4 °C
Cloud point41ºC5 g product in 25 ml 25% butyldiglycol °C
Color= 300 Hazen
Content= 97 %Tertiary Amine
Content (%)100Active content
Equivalent mass345-365
Foam Height according to Ross-Miles10 mmimmediately, 50°C, 0.05%
 5 mmafter 5 min, 50°C, 0.05%
Wetting power600 secaccording to Draves, 25°C, 0.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY528 / 286051

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.