MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total PPH 3575CC Polypropylene Homopolymer, Film Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Low Residuals TOTAL Polypropylene 3575CC utilizes the new TOTAL Polypropylene proprietary process technology to provide extremely low residuals for improved color stability and clarity.

Slip/Antiblock. 3575CC contains an optimized level of slip and antiblock additives.

FDA. 3575CC complies with all applicable FDA regulations for food contact applications.

Recommended Applications. TOTAL Polypropylene 3575CC is recommended for use in non-oriented cast film processes for manufacture of packaging films.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.905 g/cc0.905 g/ccASTM D1505
Water Vapor Transmission 10.9 g/m²/day
@Temperature 37.8 °C
0.700 g/100 in²/day
@Temperature 100 °F
90% RH; ASTM F1249-90
Melt Flow 9.0 g/10 min
@Temperature 230 °C
9.0 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.3 MPa7000 psiASTM D882
Elongation at Break 600 %600 %ASTM D882
1% Secant Modulus 483 MPa70000 psiASTM D882
Dart Drop 0.787 g/micron20.0 g/milF50; ASTM D1709
 
Thermal PropertiesMetricEnglishComments
Melting Point 163 °C325 °FDSC
 
Optical PropertiesMetricEnglishComments
Haze 2.5 %2.5 %ASTM D1003
Gloss 80 %80 %at 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 260 °C400 - 500 °FFilm Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPH 4030 Polypropylene Homopolymer
Total PPH 4026 Polypropylene Homopolymer, Film
Total PPH 3371 Polypropylene, Oriented Film Extrusion Grade
Total PPH 3962 Polypropylene Homopolymer, Ultra-High Melt Flow Rate Pelletized For Melt Blown Fiber Applications
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming

PTOTAL812 / 130537

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.