Product Description: Dowlex™ GM 8051G Polyethylene Resin is designed for use in a wide variety of film applications, in special for FFS and lamination multilayered films combining excellent optical properties, mechanicals and an additive package designed to enhance COF stability. Main Characteristics: High toughness, processability and optical properties; Fully formulated, enhanced COF stability Complies with: US FDA FCN 741 Consult the regulations for complete details. Availability: Latin America; North America Additive: Antiblock: 2500 ppm; Processing Aid: No; Slip: 900 ppm Agency Ratings: FDA FCN 741 Form: Pellets Information provided by The Dow Chemical Company |